Four application areas make up the bulk of our work. Each has its own constraints on thickness, tolerance and turnaround, so we treat them as separate problems rather than one product.
Lab work runs on iteration, not volume. You need one mask this week, a revised version next week, and you cannot wait a month for a supplier to fit you into a production schedule. This is where a three day sample turnaround actually changes what you can do.
We work from whatever you have: a proper DXF, a hand sketch with dimensions, or an existing mask you want copied with modifications.
| Material | Invar36 or stainless 304 |
|---|---|
| Thickness | 0.1 – 0.2 mm |
| Substrate size | Up to 4" wafer or custom holder |
| Position accuracy | ±20 µm |
| Quantity | 1 – 50 pieces |
| Sample lead time | 1 – 3 working days |
Evaporation has moved from an optional step to a required one in perovskite manufacturing. Electron transport layers such as C60 can only be deposited by evaporation, and textured silicon in tandem cells needs a conformal coating that only evaporation delivers. Every evaporated layer needs a mask.
On a pilot line the masks are consumables: they accumulate deposited material, get cleaned, and eventually lose edge definition. That means repeat orders, and it means the second batch has to match the first.
| Material | Invar36 |
|---|---|
| Thickness | 0.1 – 0.3 mm |
| Panel size | Coupon to large area, up to 600 × 600 mm |
| Position accuracy | ±20 – ±30 µm |
| Cycle life | Depends on process, ask us for guidance |
| Supply | Sample first, then scheduled repeat batches |
Shadow masking is still the economical answer for metallisation where photolithography is overkill or where the substrate cannot take a resist process. Wafer level masks, sensor electrode patterns and MEMS structures all fall into this bracket.
Here the requirement shifts from speed to repeatability: the mask must sit flat on the substrate, hold registration across the wafer, and survive enough cycles to make the cost per wafer sensible.
| Material | Invar36, molybdenum or nickel |
|---|---|
| Thickness | 0.1 – 0.3 mm |
| Wafer size | 2" to 8" |
| Position accuracy | ±20 µm standard |
| Flatness | Stress relieved, supplied flat |
| Documentation | Dimension report with each batch |
Filters, mirrors, photodetectors and optical waveguide structures often need patterned deposition on substrates that cannot go through a lithography line. A metal shadow mask does the job in one vacuum cycle.
| Material | Invar36 or stainless |
|---|---|
| Thickness | 0.1 – 0.5 mm |
| Feature size | From 0.1 mm depending on thickness; finer apertures by design review |
| Edge quality | Burr-free for clean shadow definition |
Selected technical notes from our engineering team.
If it involves putting a pattern into a vacuum chamber, we can probably make the mask.